Effect of Temperature on Kinetic Regularities of Forming Nanosized Particles on Steel Surface Contacting with Aqueous Dispersion Medium

Authors

  • O. M. Lavrynenko Ovcharenko Institute of Bio-Colloid Chemistry of National Academy of Sciences of Ukraine
  • V. Yu. Starchenko Ovcharenko Institute of Bio-Colloid Chemistry of National Academy of Sciences of Ukraine
  • S. V. Netreba Ovcharenko Institute of Bio-Colloid Chemistry of National Academy of Sciences of Ukraine
  • V. A. Prokopenko Ovcharenko Institute of Bio-Colloid Chemistry of National Academy of Sciences of Ukraine

Abstract

The specific character of forming nanosized structures on steel surface contacting with air and aqueous dispersion medium in the range of temperatures from 3 to 70°C has been studied. The development of iron-oxygen structures leads to morphological ?-row. As the initial structure the hydroxycarbonate Green Rust under the most conditions has been found. Two branches of phase transformation scheme under full and limited oxidation have been suggested. The optimum condition for forming lepidocrocite is low temperatures (25–35°C) and for forming magnetite is middle ones (50°C). The kinetic regularities of the XRD-pick amounts of lepidocrocite and magnetite from temperatures were calculated.

References

Prokopenko V.A., Lavrynenko E.N., Mamunya S.V The formation of nanosized iron-oxygen structures in the system FeO-H2O-O2 and ways to manage the processes of phase formation // Nanosistemy, nanomaterialy, nanotechnologii. – 2008. – V. 6, N 2. – P. 385–393.

Lavrynenko E.N., Prokopenko V.A., Lebovka N.I., Mamunya S.V. The effect of temperature on the development of nanosized nucleus iron-oxygen structures in Fe0–H2O–O2 Systems // Colloid J. – 2008. – V. 70, N 3. – P. 303–310.

Lavrynenko O.M., Korol Ya.D., Netreba S.V., Prokopenko V.A. Kinetic regularity of the formation of Fe (II)–Fe (III) LDH structures (Green Rust) on the steel surface in presence of the FeSO4 and Fe2(SO4)3 water solutions // Chemistry, Physics and Technology of Surface. – 2010. – V. 1, N 3. – P. 338–342.

Lavrynenko O.M., Netreba S.V., Prokopenko V.A., Korol Ya.D. The influence of the pH value and the cation composition of dispersion medium on the formation of iron-oxygen structures on steel surface // Chemistry, Physics and Technology of Surface. – 2011. – V. 2, N 1. – P. 93‑100.

Zozulya V.V., Lavrynenko E.N., Prokopenko V.A., Pertsev N.V. On the mechanism of processes in galvanic couple iron-carbon (coke) in aerated solution containing heavy metal ions // Ukrainskiy khimicheskiy zhurnal. – 2000. – V. 66, N 7. – P. 48–50.

Olowe A.A., Pauron B., Génin J.M.R. The influence of temperature on the oxidation of ferrous hydroxide in sulphated aqueous medium: Activation energies of formation of the products and hyperfine structure of magnetite // Corros. Sci. – 1991. – V. 32, N 9. – P. 985–1001.

Génin J.-M.R., Rézel D., Bauer Ph. et al. Mössbauer spectroscopy characterization and electrochemical study of the kinetics of oxidation of iron in chlorinated aqueous media: structure and equilibrium diagram of green rust one // Mater. Sci. Forum. – 1986. – V. 8. – P. 477–490.

Tamura H. The role of rusts in corrosion and corrosion protection of iron and steel // Corros. Sci. – 2008. – V. 50. – P. 1872–1883.

Downloads

How to Cite

(1)
Lavrynenko, O. M.; Starchenko, V. Y.; Netreba, S. V.; Prokopenko, V. A. Effect of Temperature on Kinetic Regularities of Forming Nanosized Particles on Steel Surface Contacting With Aqueous Dispersion Medium. Him. Fiz. Tehnol. Poverhni 2011, 2, 393-398.